Abstract
In this study, we have combined the ultrasonic machining with the electrochemical one. After electrochemical machining at different voltages for 3 minutes, it is seen that when the voltage increases from zero to 4 volts, the cutting depth from 0.2mm to 1.5mm (processing efficiency increase) the tool wear reduces from 0.09mm to 0.04mm. However, when at voltage of 4 volts, the toughness of the machining surface goes further. That is why the optimum voltage is in range from 2V to 3V.